O |
Min/Max |
99.95 min |
0.001 |
Nominals |
- |
- |
Product Property |
US Customary |
Metric |
Coefficient of Thermal Expansion |
9.4 @ 10 6? per °F (68-212 F) |
16.9 @ 10 6? per °C (20-100 C) |
Coefficient of Thermal Expansion |
9.6 @ 10 6? per °F (68-392 F) |
17.3 @ 10 6? per °C (20-200 C) |
Coefficient of Thermal Expansion |
9.8 @ 10 6? per °F (68-572 F) |
17.6 @ 10 6? per °C (20-300 C) |
Density |
0.323 lb/in3 @ 68 F |
8.94 gm/cm3 @ 20 C |
Electrical Conductivity |
101%IACS @ 68 F |
0.591 MegaSiemens/cm @ 20 C |
Electrical Resistivity |
10.3 ohms-cmil/ft @ 68 F |
1.71 microhm-cm @ 20 C |
Melting Point Liquid US |
1981 F |
1083 C |
Melting Point Solid US |
1981 F |
1083 C |
Modulas of Elasticity in Tension |
17000 ksi |
117000 MPa |
Modulas of Rigidity |
6400 ksi |
44130 MPa |
Specific Gravity |
8.94 |
8.94 |
Specific Heat Capacity |
0.092 Btu/lb/°F at 68 F |
393.5 J/kg @ °K at 293 K |
Thermal Conductivity |
226.0 Btu @ ft/(hr @ Ft2 @ °F) at 68 F |
391.1W/m @ °K at 20 C |