We are professional 100Cr6(AISI 52100,1.3505,SUJ2)Forging Forged Steel Rings Rolled Rings(AISI E52100,100 Cr 6) factory from china
Low alloy martensitic chrome steel, AISI 52100 thanks to its high hardness, wear resistance, surface finishing and dimensional precision, it is widely used to manufacture mechanical components.
Applications |
---|
Precision bearings, automotive components (brakes, steering, line shaft), bicycle, agitators, appliances, sliders, quick couplings, machine tool, lock mechanisms, conveyor belts, skates, pens, pumps, castors, measurement instruments, valves. |
Chemical composition
%C | %Si | %Mn | %P | %S | %Cr | - | - | - | - | - | - |
---|
0.95-1.10 | 0.35 max | 0.20-0.50 | 0.025 max | 0.025 max | 1.30-1.60 | - | - | - | - | - | - |
International standards
ITA | USA | GER | FRA | UK | RUS | CHN | JAP |
---|
100Cr6 | 52100 | 1.3505 | 100C6 | 534A99 | 9Ch1 | GCr15 | SUJ2 |
Physical / mechanical / thermal / electric / magnetic properties
Property | Symbol | U.o.M. | Type | Notes | Values |
---|
Density | δ | [g/cm3] | Physical | Room temp. | 7.80 |
Young's modulus | E | [GPa] | Mechanical | - | 200 |
Specific heat | c | [J/kg-K] | Thermal | Room temp. | 464 |
Coefficient of linear thermal expansion | α | [10^-6/ºC] | Thermal | (ΔT=0-100°C) | 12.3 |
Thermal conductivity | λ | [W/(m·K)] | Thermal | Room temp. | 42.4 |
Electric resistivity | ρ | [Ω*m*10^-9] | Electric | - | 215 |
Relative magnetic permeability | µ | - | Magnetic | Ferromagnetic | > 300 |
Technical data
Property | Type | U.o.M. | Values | U.o.M. | Values |
---|
Hardness | Mechanical | [HRC] | 60 - 66 | - | - |
Ultimate compressive strength | Mechanical | [MPa] | 2500 - 2600 | [psix10^3] | 362 - 377 |
Service temperature | Thermal | [ºC] | -60 / 150 | [ºF] | -76 / 302 |
Range
Diameters | U.o.M. | Diameters | U.o.M. | Precision Grade (ISO 3290) |
---|
0.250 - 300.000 | [mm] | 1/64 - 12 | ["] | G3-5-10-16-20-25-28-40-60-100-200-500-1000 |
Revision n. 4
The Process As Follow: ingot → heat → forging → heat treatment(normalizing+tempering) → inspection → rough machining → UT → 2nd heat treatment → finishing machining → inspection .
Quality Control: UT,MT,RT,PT,chemical composition test,mechanical property test,etc.
Heat Treatment: Normalize,Quenching,Tempering,Anealled.
Surface Treatment: painting,plating,polishing,black oxide,transparent anti-rust oil.
Inspection: Besides our in-house inspecion, you could also choose a third party inspection.
Standard: ANSI,ASTM,ASME,API,JIS,DIN,BS,EN,KS,UNI,SABS,GOST.
Certificate: 1, Raw material certificate(material chemical compositon)
2, Heat treatment sheet report
3, Dimension inspection report
4, UT test report
Packing: Seaworthy plywood packaged on stell pallets or as customer's request
Delivery Date: Decided by the amount and dimensions of products. Usually we control the large diameter rings' delivery time within 5 weeks after we receive your formal order.
Competitive Advantage: Quality control and management to the whole produce process, including ingot smelting,forging, heat treatment, machining and strictly final inspection prior to delivery.